Fused Glass Picture Frame

By Alison Morris

  • Art
  • Senior
Activity Time
Three of four classroom sessions
Concepts / Topics
Students will work with color and shapes to creat an abstract look

Students cut and arrange glass strips and frit into a frame design, fire it in a kiln, then glue it to an acrylic frame; the resource also provides glass-fusing rules and schedules.

Objectives

Students will learn glass cutting to create a “mosaic look” picture frame, work with color and shape to create abstract designs, and learn fusing and kiln basics.

Grade Level and Time Required

High school. Three to four sessions.

Materials for 12 Projects

QuantityItem NumberDescription
3 sm#B110150Clear glass (cut into ¾″ × 3½″ strips)
1#F790190Golden Amber Mosaic Frit
1#F770190Evergreen Mosaic Frit
1#F740390Cobalt Blue Mosaic Frit
1#F760690Red Mosaic Frit
12Acrylic frames, 3.5″ × 5″ (available from most craft or photo stores)
1#LN275Adhesive glue

Glass Cutting Supplies

  • 1 #5104 Toyo Glass Cutter
  • 1 #5068 Running Pliers
  • 1 #5163 Safety Glasses

Teacher’s note: One sheet of clear glass strips makes twelve frames. One bottle of each of the mosaic frits makes about 12+ frames. Use extra sheets of clear glass to make additional frames. Students can also use fusible glass instead of frit to create their own design.

Directions

Refer to Delphi’s Instructions for Fusing for detailed instructions.

  1. Cut clear glass into strips. For glass cutting directions, see the Delphi Instructions for Beginning Stained Glass handout or Stained Glass Made Easy video #6149V.
  2. On a kiln-washed shelf, arrange the clear strips to form a rectangle.
  3. Cover the clear glass with random pieces of mosaic frit. It is acceptable to overlap the colors.
  4. Using the fusing schedule in Delphi’s Instructions for Fusing, place in the kiln and fire flat.
  5. Attach a clear acrylic frame to the back of the fused picture frame with adhesive glue. Insert your favorite photo!

Tip: Be sure there are at least two layers of glass over each of the seams, or you may get a hole.

Photography and project from Glass Fusing Made Easy book #5981. Please refer to it for more detailed directions and beautiful beginner projects.

Glass Fusing Rules and Firing Instructions

Fusing glass in a kiln is a fascinating technique that enables artists to create unique and gorgeous projects. The following fusing rules and firing instructions should provide you with enough information to lead your students through a variety of projects, creating an appreciation for the complexities and potential of fused glass, and paving the way for more intricate designs and ideas.

Tested Compatible

  • A. All glass has a coefficient of expansion, or COE.
  • B. Glass manufactured specifically for fusing is often “tested compatible,” or guaranteed to be a certain COE.
  • C. The most popular fusing glasses are either 90 COE (Bullseye, Uroboros, Wasser) or 96 COE (Spectrum and Uroboros).
  • D. Always use compatible glass, which is known to have the same COE.

When glass is heated, it expands; when it cools, it contracts. If fusing two or more pieces of glass together, they need to expand and contract at the same rate. Otherwise, when the glass cools, one glass will pull on the other and cause the piece to crack along the seam.

If the glass survives the cooling process, there is still a risk that reheating to bend it or placing it in a sunny window will cause cracking. Stress from incompatible glass is always in the piece. Do not try to refire broken incompatible glass.

Slower Is Better

You can’t heat or cool glass too slowly. Going too fast can result in cracked glass or thermal shock (photo 1).

A safe rate to heat is 15° per minute (900° per hour), although stacked glass 2″ in diameter and smaller can be heated at a faster rate.

Slow cooling of glass, or “annealing,” depends on the thickness of the glass. If the glass breaks because it was heated too fast, turn off the kiln, allow the glass to cool, push it back together, and try again—at a slower rate. Breaks from thermal shock usually go straight across the piece and have a little hook near the edge. They can usually be repaired by refiring.

Glass Likes to Be ¼″ Thick

When heating glass to full fuse, anything with less mass will shrink up; anything with more will spread out. This movement can be controlled somewhat by fusing slower and not going to full fuse.

All Kilns Are Not Alike

  • A. There are some variances between kilns, especially mini kilns. Sometimes pyrometers are slightly off, and sometimes current loads vary.
  • B. Use firing schedules as a guide, but remember to check your piece frequently during fusing, and record changes in schedules as needed.
  • C. Prepare your kiln by applying kiln wash with a kiln brush. Apply one thin coat in each direction. Don’t forget to apply kiln wash to molds, too.

Take Good Notes

  • A. Use a project log to keep important information about your projects.
  • B. Keep track of what glass was used, how thick the glass was, the firing schedule and the results.
  • C. This helps repeat good performances and prevent bad ones.

Fusing Glass

Glass Fusing Stages for Mini Kilns

Common TemperaturesFusing StageGlass Stages
800°F–1100°FBrittle ZoneDo not open the kiln in this range.
1325°F–1425°FTack FuseEdges are soft; glass is stuck together (photo 2).
1425°F–1600°FFull FuseGlasses combine; uniform thickness throughout (photo 3).

Fusing Schedule

Use for tabletop kilns, pieces ¼″ thick and 3″–6″ in diameter. Larger pieces should be heated and cooled slower to prevent thermal shock.

Dial Setting and TimeKiln TemperatureGlass Stage
2 for 20 minutes (check kiln)About 500°FNo change in glass
3 for 30 minutes (check kiln)About 1000°FStill no change in glass
4 for 10 minutes (check kiln)About 1500°FGlass should be slightly more than tack fused
4 for 5 minutes (check kiln)About 1500°FGlass should be full fused (see further instructions below)

When the Desired Look Has Been Achieved

Turn off the kiln.

  1. To stop the fusing process, flash vent the glass to let the heat out by holding the lid off the kiln about 8 seconds and watching the glass surface turn from orange to blackish (the color will return to the glass as it cools). Repeat the process until the temperature stays close to 1000° when the lid is replaced.
  2. Replace the lid and turn the kiln on low for 20 minutes. This will keep the kiln approximately 1000–1200°, allowing a minimal annealing cycle. Turn off the kiln and cool naturally to room temperature.

If More Melting Is Desired

Turn the dial to 5, but do not leave the kiln.

  1. It is easy to overfire glass at this temperature and ruin the piece. Let the kiln heat to 1600° and turn the dial back to 4. This will allow the kiln to get slightly hotter without continuing to gain heat.
  2. Check the piece every 3 minutes and try not to let the kiln go above 1600°. When the desired look is achieved, follow the instructions above.

Basic Supplies

Listed with Delphi item numbers for quick reference

  • #HB120 Table Top Kiln
  • #7441 Ceramic Kiln Shelf — 6″
  • #7465FM Kiln Wash
  • #7466 Haik Brush
  • #FIREUPS Tested compatible glass — Uroboros Glass Pack, 90 COE
  • Glass Cutting Supplies

    • #5104 Glass Cutters
    • #5068 Running Pliers
    • #5066 Breaker/Grozer Pliers
  • Variety of Bending Molds

    • #7433 4¼″ Shallow Dish Mold
    • #J4 Belt Buckle/Barrette Mold

Kiln Parts

All glass fusing kilns have basically the same parts:

  • Elements (high-temperature coiled wire)
  • Firebrick insulation
  • Stainless steel cover
  • Thermocouple (high-temperature wires covered by ceramic rings)
  • Pyrometer (temperature readout dial)
  • Infinite Dial — some kilns simply have an on/off switch; the Hot Box pictured has the Infinite Dial.

Credits and Further Resources

Photography and instructions from Glass Fusing Made Easy book #5981. For more information and project ideas refer to this book and Delphi’s fusing favorites:

Fused Glass Handbook #6430

Fusing guru Gil Reynolds presents 25 projects with easy-to-follow instructions for mold-making, creating pattern bars, and many other hot glass techniques.

Kiln Crafted Video #4990V

Discover how glass shaping techniques developed thousands of years ago have been put to use by contemporary artists. Observe different stages of the glass melting process. Learn how to turn ordinary glass into beautiful sculpture, as well as forming, mold materials, preparation, heating and cooling cycles, and more. Includes example projects ranging from beginner levels to advanced.